TY - JOUR T1 - Shear Bond Strength of Reused Orthodontic Brackets after Multiple Bonding Cycles: An in Vitro Study A1 - Su'ud Basaad A1 - Johan Arief Budiman A1 - Octarina Octarina JF - Asian Journal of Periodontics and Orthodontics JO - Asian J Periodontics Orthod SN - 3062-3499 Y1 - 2026 VL - 6 IS - 1 DO - 10.51847/LocQtMgOTb SP - 25 EP - 31 N2 - Repeated bonding of orthodontic brackets is a common clinical necessity, yet its impact on shear bond strength (SBS) and enamel integrity remains inadequately characterized. This study evaluated the effect of multiple bonding cycles using the same bracket on SBS and enamel surface characteristics. Twenty human premolars extracted for orthodontic purposes were randomly allocated to two groups (n=10 per group): Group A (Enlight® adhesive, Ormco) and Group B (Transbond XT® adhesive, 3M Unitek). Specimens underwent five consecutive bonding-debonding cycles using stainless steel mesh-based brackets. After each debonding, brackets were cleaned using a flaming technique (5 seconds), and enamel surfaces were polished with a tungsten carbide bur. SBS was measured using a universal testing machine (crosshead speed: 6 mm/min). Data were analyzed using repeated measures MANOVA with Bonferroni post hoc tests (α=0.05). Initial SBS values differed significantly between groups (Group B: 22.38±17.41 MPa vs. Group A: 9.92±4.36 MPa; p UR - https://tsdp.net/article/shear-bond-strength-of-reused-orthodontic-brackets-after-multiple-bonding-cycles-an-in-vitro-study-pmlluvsgrbysj59 ER -